Ribbon Backing and Substrate Materials: How Construction Changes Cost, Drape and Print Adhesion

Published: 2026-11-26  |  Updated: 2026-11-26  |  By Xiamen Smith Ribbon & Bow Co., Ltd.  |  Since 2004

A brand buyer comparing two ribbons that look identical in a swatch book is very often looking at two different products. The face fabric may be the same fibre, the same width and the same colour, but the backing can differ entirely — and the backing is what determines whether the ribbon is a flat decorative trim, a structural element, a fusible component or a self-adhesive product.

Because the face is what is visible, the backing is what gets specified last and discussed least. That is a mistake with long consequences, because the backing is where a surprising number of the practical failures originate. Print that flakes because the ink could not key into the backing. Ribbon that curls because the backing and the face have different coefficients of thermal expansion. A gift bow that loses its shape because the backing was too stiff. A price that arrives at landed cost well above the quoted figure because the backing adds weight, and weight is what freight charges on.

The useful mental model is that a ribbon is a composite. The face provides appearance, colour and hand-feel. The backing provides structural behaviour, dimensional stability, bondability and, quite often, a large share of the cost. Treating them as a single specification item means you cannot diagnose a failure, because you do not know which layer caused it.

Ribbon OEMB2B ProcurementSmith Ribbon since 2004

Why the backing deserves its own line on the specification

A brand buyer comparing two ribbons that look identical in a swatch book is very often looking at two different products. The face fabric may be the same fibre, the same width and the same colour, but the backing can differ entirely — and the backing is what determines whether the ribbon is a flat decorative trim, a structural element, a fusible component or a self-adhesive product.

Because the face is what is visible, the backing is what gets specified last and discussed least. That is a mistake with long consequences, because the backing is where a surprising number of the practical failures originate. Print that flakes because the ink could not key into the backing. Ribbon that curls because the backing and the face have different coefficients of thermal expansion. A gift bow that loses its shape because the backing was too stiff. A price that arrives at landed cost well above the quoted figure because the backing adds weight, and weight is what freight charges on.

The useful mental model is that a ribbon is a composite. The face provides appearance, colour and hand-feel. The backing provides structural behaviour, dimensional stability, bondability and, quite often, a large share of the cost. Treating them as a single specification item means you cannot diagnose a failure, because you do not know which layer caused it.

A brand buyer comparing two ribbons that look identical in a swatch book is very often looking at two different products. The face fabric may be the same fibre, the same width and the same colour, but the backing can differ entirely — and the backing is what determines whether the ribbon is a flat decorative trim, a structural element, a fusible component or a self-adhesive product.

Because the face is what is visible, the backing is what gets specified last and discussed least. That is a mistake with long consequences, because the backing is where a surprising number of the practical failures originate. Print that flakes because the ink could not key into the backing. Ribbon that curls because the backing and the face have different coefficients of thermal expansion. A gift bow that loses its shape because the backing was too stiff. A price that arrives at landed cost well above the quoted figure because the backing adds weight, and weight is what freight charges on.

The four backing families and what each one does

Backing familyStructureDrape and stabilityBest suited to
Self-woven selvedgeSame yarn system as the face, woven to a firm edgeVery stable, moderate stiffness, clean edgeStructural trim, bows, gift wrapping where edge quality matters
Woven fabric backingSeparate plain-weave or taffeta fabric laminated to the faceStable, heavier, can be engineeredHeavy decorative ribbons, wide formats, items needing body
Film backingMetallised, opaque or translucent film laminated to the faceVery stable, smooth surface, distinctive handMetallic and glitter effects, reflective formats, high-shimmer decorative
Nonwoven or foam backingBonded fibre web or foam layerSoft, cushioned, low structureElastic applications, gift wrap cushioning, craft formats
Adhesive backingHeat-activated or pressure-sensitive adhesive layerAs face, but bonded on useGarment and home textile appliqué, no-sew installation

Self-woven selvedge: the default, and what it hides

Most ordinary ribbon is self-woven. The warp and weft yarns that form the face continue into the edge, and the edge is finished either by folding or by a separate weft binding. The result is a ribbon whose edge will not fray and whose width is stable, because the whole thing is one piece of cloth.

The advantage is coherence. There is no second material to disagree with the face, no delamination risk, no differential shrinkage between layers, and no adhesive to fail. It is also the most economical construction and the one with the broadest colour and width availability, because it is what the mills are set up to make.

The limitation is that the edge quality is a function of the weave. A narrow ribbon woven for 10mm has a proportionally large edge relative to its width, and the fold or binding that finishes it becomes visually significant. Buyers who want a genuinely crisp edge on a narrow ribbon are usually looking at a wider loom configuration or a different construction, and this is worth understanding before requesting a sample, because "make the edge better on a 9mm ribbon" is a change to the weaving plan, not a finishing tweak.

On a self-woven ribbon, the face yarn and the edge are integrated, so there is no separate backing surface for the ink to sit on. This is generally an advantage for print adhesion, because the ink keys into the yarn structure rather than sitting on a smooth film. It also means the print follows the weave, which is exactly what you want for a brand mark that must not crack or peel when the ribbon is bent around a bow.

Most ordinary ribbon is self-woven. The warp and weft yarns that form the face continue into the edge, and the edge is finished either by folding or by a separate weft binding. The result is a ribbon whose edge will not fray and whose width is stable, because the whole thing is one piece of cloth.

The advantage is coherence. There is no second material to disagree with the face, no delamination risk, no differential shrinkage between layers, and no adhesive to fail. It is also the most economical construction and the one with the broadest colour and width availability, because it is what the mills are set up to make.

The limitation is that the edge quality is a function of the weave. A narrow ribbon woven for 10mm has a proportionally large edge relative to its width, and the fold or binding that finishes it becomes visually significant. Buyers who want a genuinely crisp edge on a narrow ribbon are usually looking at a wider loom configuration or a different construction, and this is worth understanding before requesting a sample, because "make the edge better on a 9mm ribbon" is a change to the weaving plan, not a finishing tweak.

The selvedge construction matters for print registration

Woven fabric backing: engineering the ribbon's behaviour

A woven fabric backing — plain weave, taffeta, or a heavier construction — is laminated to the ribbon face. This is how you get body into a ribbon that would otherwise be limp: it gives a wide decorative ribbon the stiffness to stand in a bow, to hold a fold in a gift bag, or to form a structured rosette.

Because the backing is a separate engineered material, this route gives you control that self-woven cannot. It is the standard answer when the ribbon has a structural function rather than a decorative one, and it is where the trade-offs become sharp.

Weight is the cost. A backed ribbon weighs substantially more per metre than the same face unbacked. This affects two things at once: the material cost per metre, and the freight. Ribbon ships volumetrically, and freight is charged on the space a carton occupies rather than strictly on its weight — but weight still drives the carton density, and a heavier product at the same roll length means fewer metres per carton, which means more cartons for the same order. A ribbon that looks like a small price increase per metre can carry a disproportionate freight increase per delivered carton.

Drape changes, and that is often the point. A backed ribbon hangs differently. In a boutique retail presentation, in a gift box where the ribbon must hold an architectural fold, or in a wreath where the ribbon must stand away from the surface, this is the entire purpose of the backing. But in a soft drape application, a heavily backed ribbon can look wrong, and buyers who are surprised by this usually are because nobody specified the intended handling.

Edge quality must be specified separately. A backed ribbon has a composite edge, and that edge is usually finished by folding or by an over-lock stitch. If the edge is visible in the finished product, say so. Edge finish is a design decision, and it is the part of a backed ribbon that most often looks wrong in a finished assembly.

A woven fabric backing — plain weave, taffeta, or a heavier construction — is laminated to the ribbon face. This is how you get body into a ribbon that would otherwise be limp: it gives a wide decorative ribbon the stiffness to stand in a bow, to hold a fold in a gift bag, or to form a structured rosette.

Because the backing is a separate engineered material, this route gives you control that self-woven cannot. It is the standard answer when the ribbon has a structural function rather than a decorative one, and it is where the trade-offs become sharp.

Weight is the cost. A backed ribbon weighs substantially more per metre than the same face unbacked. This affects two things at once: the material cost per metre, and the freight. Ribbon ships volumetrically, and freight is charged on the space a carton occupies rather than strictly on its weight — but weight still drives the carton density, and a heavier product at the same roll length means fewer metres per carton, which means more cartons for the same order. A ribbon that looks like a small price increase per metre can carry a disproportionate freight increase per delivered carton.

Drape changes, and that is often the point. A backed ribbon hangs differently. In a boutique retail presentation, in a gift box where the ribbon must hold an architectural fold, or in a wreath where the ribbon must stand away from the surface, this is the entire purpose of the backing. But in a soft drape application, a heavily backed ribbon can look wrong, and buyers who are surprised by this usually are because nobody specified the intended handling.

Film backings: the metallic and glitter family

A metallised film — aluminium, or a metallised polyester film — laminated to a ribbon face is what produces the high-shimmer metallic ribbons used across gift packaging and holiday decoration. The film carries the reflective surface, and the face beneath provides the colour or the printed artwork. Sometimes the film is on the reverse and the printed face is on top; sometimes the film is the visible surface itself.

These constructions come with two distinctive characteristics that a buyer needs to understand before ordering.

Metallised film is a mirror, and it reflects the environment. A metallised surface shows the room around it. Under warm retail lighting it reads warmer; under cool light it reads cooler; under direct sun it can look almost white at the highlight. This is not a defect and it cannot be corrected by a better colour match, but it does mean that a metallic ribbon cannot be colour-approved in a swatch the way a dye-based ribbon can. The right process is a physical sample viewed in the actual lighting of the retail environment, and ideally photographed there, because photographs reproduce the environment of the photographer.

Adhesion between film and face is a bond, and bonds fail at the folds. This is the single most important practical fact about film-backed ribbon. A film laminate is held to the face by an adhesive layer, and the failure mode is not gradual: the film delaminates, typically beginning at a crease, a fold, or the point where the ribbon has been bent tightly around a bow. It looks dramatic — a silver skin peeling away from a printed surface — and it is a frequent reason for returns on metallic ribbon used in gift bows, where every bow is a tight bend.

The cure is in the specification, not in the product. Specify the peel strength of the film bond, specify the minimum bend radius the product is expected to withstand, and specify that the assembly must be tested in its finished form. A metallic ribbon that is perfectly adequate on a spool can be entirely unsuitable for a pre-tied bow.

A metallised film — aluminium, or a metallised polyester film — laminated to a ribbon face is what produces the high-shimmer metallic ribbons used across gift packaging and holiday decoration. The film carries the reflective surface, and the face beneath provides the colour or the printed artwork. Sometimes the film is on the reverse and the printed face is on top; sometimes the film is the visible surface itself.

These constructions come with two distinctive characteristics that a buyer needs to understand before ordering.

Metallised film is a mirror, and it reflects the environment. A metallised surface shows the room around it. Under warm retail lighting it reads warmer; under cool light it reads cooler; under direct sun it can look almost white at the highlight. This is not a defect and it cannot be corrected by a better colour match, but it does mean that a metallic ribbon cannot be colour-approved in a swatch the way a dye-based ribbon can. The right process is a physical sample viewed in the actual lighting of the retail environment, and ideally photographed there, because photographs reproduce the environment of the photographer.

Adhesion between film and face is a bond, and bonds fail at the folds. This is the single most important practical fact about film-backed ribbon. A film laminate is held to the face by an adhesive layer, and the failure mode is not gradual: the film delaminates, typically beginning at a crease, a fold, or the point where the ribbon has been bent tightly around a bow. It looks dramatic — a silver skin peeling away from a printed surface — and it is a frequent reason for returns on metallic ribbon used in gift bows, where every bow is a tight bend.

Nonwoven and foam backings: soft structures with a different set of rules

Nonwoven and foam backings sit at the opposite end of the stiffness spectrum. A nonwoven-backed ribbon is soft, light, forgiving and cheap; it is used where a ribbon needs to sit flat against a surface, or as a base layer under printed organza and sheer effects. Foam-backed ribbon has volume and a cushioned hand, which is the basis of many craft and gift formats.

Two issues recur. The first is dimensional stability: a foam or nonwoven layer compresses under pressure, so a ribbon wound on a tight roll can show a compression set, and the compression can differ across a roll depending on how it was wound and how it has been stored. The second is surface interaction: because these backings are soft and porous, adhesive-backed application and any form of heat application need testing, and a nonwoven-backed ribbon is generally a poor candidate for fusible installation without a specific test.

Nonwoven and foam backings sit at the opposite end of the stiffness spectrum. A nonwoven-backed ribbon is soft, light, forgiving and cheap; it is used where a ribbon needs to sit flat against a surface, or as a base layer under printed organza and sheer effects. Foam-backed ribbon has volume and a cushioned hand, which is the basis of many craft and gift formats.

Adhesive-backed ribbon: a specification in a different language

Adhesive-backed ribbon — heat-activated fusible, or pressure-sensitive — changes the product from a decorative trim into an installation component. The buyer is no longer specifying a material; they are specifying a system with a process, a temperature window, a press time and a bond result.

Everything that is routine for an unbacked ribbon becomes a variable for an adhesive-backed one.

The heat window is narrow. A fusible adhesive needs enough heat and pressure to activate, and enough time. Too little and the bond is incomplete; too much and the adhesive bleeds through the face, the colour shifts, the face scorches, or the ribbon shrinks because the face has been exposed to more heat than it tolerates. Ribbon faces differ in their heat tolerance — a polyester ribbon tolerates considerably more than a delicate sheer organza — and the process window must be set for the specific ribbon, not taken from a generic recommendation.

Bond strength varies by face and construction. The same adhesive behaves differently on a woven selvedge ribbon, on a soft nonwoven, and on a film-backed metallic. The bond failure will occur at the weakest interface, which is often not where anyone expects it.

Wash and heat durability are separate questions from bond strength. An adhesive can achieve an excellent initial bond and still be unsuited to a garment that will be laundered. If the ribbon will be washed, the bond must be specified for wash durability as well as for initial peel strength, and the two are different tests.

When specifying adhesive-backed ribbon, the specification must include the adhesive type and its technical datasheet, the recommended heat, pressure and dwell time, the bond-strength requirement, any wash or care requirement, and the ageing conditions. A supplier who cannot give you those is not going to give you a consistent bond on your production line either.

Adhesive-backed ribbon — heat-activated fusible, or pressure-sensitive — changes the product from a decorative trim into an installation component. The buyer is no longer specifying a material; they are specifying a system with a process, a temperature window, a press time and a bond result.

Everything that is routine for an unbacked ribbon becomes a variable for an adhesive-backed one.

The heat window is narrow. A fusible adhesive needs enough heat and pressure to activate, and enough time. Too little and the bond is incomplete; too much and the adhesive bleeds through the face, the colour shifts, the face scorches, or the ribbon shrinks because the face has been exposed to more heat than it tolerates. Ribbon faces differ in their heat tolerance — a polyester ribbon tolerates considerably more than a delicate sheer organza — and the process window must be set for the specific ribbon, not taken from a generic recommendation.

Bond strength varies by face and construction. The same adhesive behaves differently on a woven selvedge ribbon, on a soft nonwoven, and on a film-backed metallic. The bond failure will occur at the weakest interface, which is often not where anyone expects it.

Wash and heat durability are separate questions from bond strength. An adhesive can achieve an excellent initial bond and still be unsuited to a garment that will be laundered. If the ribbon will be washed, the bond must be specified for wash durability as well as for initial peel strength, and the two are different tests.

How the backing changes the cost and the landed basis

Backing affects cost in three distinct ways, and buyers routinely look at only the first.

The direct material cost of the backing itself, and of the lamination process that bonds it to the face. Film-backed metallic ribbon costs more than an unbacked printed ribbon because of the metallised film, which is a significant fraction of the material cost.

The yield, which is where backing quietly hurts. A ribbon that is stiffer or thicker limits how many metres fit on a roll of a given core diameter, and it changes the carton configuration. Backed ribbon typically runs longer on the roll than the equivalent unbacked ribbon at the same width, which partly offsets the material cost and partly does not.

The freight, which is affected by both the weight and the volume. This is the component that most often breaks the expectation set by the per-metre price. A buyer comparing a backed ribbon to an unbacked one on a price-per-metre basis is often comparing a product that will fill a carton differently, and the true comparison is per delivered metre per delivered carton, which means including freight, duty and the cost of the packaging itself.

The right comparison basis is the landed cost of the same functional deliverable: the same number of metres of usable ribbon, in the same carton format, at the destination, with the same yield and waste allowance. A mill that quotes only per-metre at the factory gate is quoting a number you cannot act on, however attractive it looks.

Backing affects cost in three distinct ways, and buyers routinely look at only the first.

The direct material cost of the backing itself, and of the lamination process that bonds it to the face. Film-backed metallic ribbon costs more than an unbacked printed ribbon because of the metallised film, which is a significant fraction of the material cost.

The yield, which is where backing quietly hurts. A ribbon that is stiffer or thicker limits how many metres fit on a roll of a given core diameter, and it changes the carton configuration. Backed ribbon typically runs longer on the roll than the equivalent unbacked ribbon at the same width, which partly offsets the material cost and partly does not.

The freight, which is affected by both the weight and the volume. This is the component that most often breaks the expectation set by the per-metre price. A buyer comparing a backed ribbon to an unbacked one on a price-per-metre basis is often comparing a product that will fill a carton differently, and the true comparison is per delivered metre per delivered carton, which means including freight, duty and the cost of the packaging itself.

Specification clauses that prevent the common failures

A workable backing specification includes the following.

  1. The backing type, named precisely. Self-woven selvedge with the edge construction described, or woven fabric backing with the fibre and construction, or film with the material and metallisation type, or adhesive with the chemical type and technical datasheet reference.
  2. The lamination method and its location. Whether lamination happens at the mill or at a separate converter, and who owns the process. A composite ribbon laminated by a third party has a different failure attribution than one laminated in-house.
  3. Bond performance where a bond exists. Peel strength in the unit and condition the supplier reports, plus the bend radius or cycle count the product must survive. For film-backed and adhesive-backed ribbon this is not optional.
  4. Dimensional tolerances on the finished product, including width, thickness where relevant, and the width tolerance after lamination, which is not always the same as the face tolerance.
  5. Edge construction and finish where the edge is visible, including the cut or fold and whether the edge is bound, over-locked or raw.
  6. Colour approval for metallised surfaces by physical sample in the destination lighting, since a metallised surface cannot be approved by reference to a printed swatch alone.
  7. Storage and ageing conditions for the product, and the shelf-life expectation, particularly relevant to foam and nonwoven backings.
  8. Requalification triggers for any change to the face fibre, backing material, adhesive type, lamination supplier or lamination process, since every one of these changes the composite and can change the performance.

A workable backing specification includes the following.

How to ask a supplier the right questions

The conversation should be about the composite rather than the ribbon. A useful set of questions includes the following.

Can you describe the construction of the ribbon I am buying, face and backing separately? What is the lamination method, and where does it happen? What is the bond specification for a film-backed or adhesive-backed construction, and is it tested on the finished assembly or on flat stock? What does the peel strength become after the product has been bent around a bow? How does the backed version differ from the equivalent unbacked ribbon in metres per carton and in freight weight? What is the wash durability of the adhesive, if the application is laundered? What happens if I ask for a different backing on the same face, and what changes in price and lead time?

The quality of the answers tells you something about the supplier. A supplier who can describe the composite construction precisely, quote the bond data without hedging, and explain how the backing changes the logistics has an engineering process behind the product. A supplier who can only discuss the face is a supplier who is buying the backing in — which may be perfectly fine, but you should know it before you write the specification.

The conversation should be about the composite rather than the ribbon. A useful set of questions includes the following.

Can you describe the construction of the ribbon I am buying, face and backing separately? What is the lamination method, and where does it happen? What is the bond specification for a film-backed or adhesive-backed construction, and is it tested on the finished assembly or on flat stock? What does the peel strength become after the product has been bent around a bow? How does the backed version differ from the equivalent unbacked ribbon in metres per carton and in freight weight? What is the wash durability of the adhesive, if the application is laundered? What happens if I ask for a different backing on the same face, and what changes in price and lead time?

Working with a mill that builds the composite itself

At a vertically integrated mill the backing decision sits with the same organisation that weaves, dyes, prints and converts the ribbon, which shortens the loop considerably. Specification changes, sample rounds and corrective actions happen without a translation step between three or four companies, and the quality record for the face and the backing lives in one place.

That matters most at exactly the moments when problems are hardest: a new colourway that needs a different backing, a decoration that will not bond to a film and needs a woven alternative, a bonding problem on the customer's line that turns out to be a process window issue. These are the cases where the value of an integrated supply chain is not theoretical.

Smith Ribbon & Bow has built woven, printed, velvet, satin, organza and RPET ribbons in Xiamen since 2004, from a 15,000 m² plant with 200+ staff and 100,000 m daily capacity, holding OEKO-TEX®, GRS, FSC, BSCI, SEDEX, ISO 9001 and SMETA. If you are specifying a backed or laminated ribbon and want to understand the construction options, ask for a sample pack and a written recommendation on the backing for your specific assembly — that conversation is usually more valuable than a swatch book.

At a vertically integrated mill the backing decision sits with the same organisation that weaves, dyes, prints and converts the ribbon, which shortens the loop considerably. Specification changes, sample rounds and corrective actions happen without a translation step between three or four companies, and the quality record for the face and the backing lives in one place.

That matters most at exactly the moments when problems are hardest: a new colourway that needs a different backing, a decoration that will not bond to a film and needs a woven alternative, a bonding problem on the customer's line that turns out to be a process window issue. These are the cases where the value of an integrated supply chain is not theoretical.

Frequently Asked Questions

What is the difference between a self-woven ribbon and a backed ribbon?

A self-woven ribbon is one piece of cloth, with the edge formed from the same yarns as the face, so there is no separate layer and no risk of the backing separating. A backed ribbon has a second material bonded to the face, which is how you add body, stiffness, bondability or a metallic surface. The composite version is more controllable in structural terms, but it introduces a bond that has to be specified and tested, and it changes the weight, the roll length and the freight.

Why does metallised ribbon look different in different shops?

A metallised surface reflects the light around it rather than absorbing it, so under warm retail lighting it reads warm, under cool lighting it reads cool, and under direct daylight the highlights can look nearly white. This is a physical property of a mirror-like surface, not a colour fault, and it cannot be resolved by a closer colour match. The correct approval method is a physical sample viewed in the lighting of the environment where it will be sold, ideally with photographs taken there as well.

Why is my metallic ribbon peeling away from the printed face after it is made into bows?

Because the film laminate is held on by an adhesive bond, and the failure starts at the point of maximum stress, which is the tight bend where the ribbon is folded into a bow. A ribbon that performs perfectly on a spool can fail once it is bent, because the bend radius is far tighter than the flat-stock test ever reproduces. The fix is in the specification: state the bond peel strength, state the minimum bend radius or cycle count the assembly must survive, and require the bond to be tested on the finished assembly rather than on flat ribbon.

Does a heavier backing meaningfully change the freight cost?

Yes, more than most buyers expect, and for two reasons. Backed ribbon is heavier per metre, and it usually changes the metres per roll and therefore the carton configuration, so the volume and density of what ships both shift. The right way to compare is landed cost per delivered metre in the carton format you will actually receive, rather than price per metre at the factory gate, because the factory-gate number excludes freight, duty and packaging entirely.

Can I get the same face ribbon with different backings?

Usually yes, and it is a question worth asking early because the backing changes the product rather than merely finishing it. Switching from a self-woven construction to a woven fabric backing adds body and stiffness and changes the price, the lead time and the metres per carton. Switching to an adhesive backing changes the product into an installation component with a defined heat, pressure and dwell window. Give the supplier the end use and the assembly method rather than a backing name, and ask what they would recommend.

How should I specify an adhesive-backed ribbon?

Specify it as a system rather than a material: the adhesive type with a technical datasheet reference, the recommended heat, pressure and dwell time, the required bond strength, any wash or care requirement, and the ageing conditions the bond must survive. Initial peel strength and wash durability are different tests, and a bond that is excellent on the bench and inadequate on a laundered garment is a common and entirely avoidable outcome.

Is it worth specifying the edge finish on a backed ribbon?

Whenever the edge is visible, and on a backed ribbon it usually is, because the composite edge is finished by folding or over-locking and behaves differently from a self-woven selvedge. A stiff backed ribbon needs a different edge treatment from a soft one, and a metallic laminate makes any edge treatment more visible. The edge of a ribbon is the part of the product that the customer handles, so it is worth a specific clause rather than a default.

What happens to the certification if the backing changes?

It normally has to be reconsidered, and this is one of the most commonly missed requalification triggers. Many of the certificates that matter for ribbon — chemical compliance, flammability behaviour, in some cases fibre-content and origin declarations — depend on the whole construction rather than the face alone, because the backing contributes material to the article. Changing the backing, the lamination adhesive, the lamination supplier or the lamination process should be written into the specification as a trigger for re-testing and re-approval.

Ready to source ribbons and bows with a mill that answers the hard questions?

Smith Ribbon & Bow has supplied woven, printed, velvet, satin, organza and RPET ribbons to brand buyers in over 50 countries since 2004 — from a 15,000 m² plant with 200+ staff and 100,000 m daily capacity, holding OEKO-TEX®, GRS, FSC, BSCI, SEDEX, ISO 9001 and SMETA.

Request a quotation or a sample pack →  |  Browse the ribbon guides →